INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

7079-T6 properties
2

7079-T6 properties

7079-T6 properties

(OP)
I'm looking for information on alloy 7079-T6 material properties.  From what I have been able to find online, this material is for extrusions and is considered "obsolete".  Any information would be greatly appreciated.

"Art without engineering is dreaming; Engineering without art is calculating."

Have you read FAQ731-376: Eng-Tips.com Forum Policies to make the best use of Eng-Tips Forums?

RE: 7079-T6 properties

Aluminium Bars, Rods, Wire, Hot rolled, or Cold drawn, Tubing, Forged Rings or Forgings made of UNS A97079
http://www.stephan-stahl.de

RE: 7079-T6 properties

You can find all the mechanical properties in the older versions of Mil-Hndbk-5. I know it is in 5B and 5C.

RE: 7079-T6 properties

(OP)
Crackman, thanks for that reference, I will try to dig one up.

40818, that's as close as I'll probably get.  Thank you.

It seems this material only comes in plate form.  My customer is requiring this material for a 5.00" diameter part.

"Art without engineering is dreaming; Engineering without art is calculating."

Have you read FAQ731-376: Eng-Tips.com Forum Policies to make the best use of Eng-Tips Forums?

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources