INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

flange pressure ratings for A182 F316LN

flange pressure ratings for A182 F316LN

flange pressure ratings for A182 F316LN

(OP)
I need to find working pressure data for a flange material.  It is A182F316LN.  B16.5 does not list this material.  I see the material in other ASME publications so I believe it to be a legitimate material.  Any help would be appreciated.
thanks
Mark

RE: flange pressure ratings for A182 F316LN

Comparing in ASTM A 182 the nickel range is more narrow (11-14%) than permitted for 316L (10-15%)and nitrogen content is higher, up to 0.10% for 316L and between 0.10% and 0.16%.  I don't know what the nitrogen content might affect.

RE: flange pressure ratings for A182 F316LN

pipe15,
Refer ASME II-D, for the material ASME SA182-316LN (S31653), listed as acceptable material for use as forged flange in nuclear pressure vessel design (ASME III), up to some 430 deg C.
cheers,
gr2vessels

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources