thermal spray coating to prevent polythionic acid SCC
thermal spray coating to prevent polythionic acid SCC
(OP)
Has anyone attempted to use a thermal spray coatings lto minimize polythionic acid stress corrosion cracking?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
thermal spray coating to prevent polythionic acid SCC
|
RE: thermal spray coating to prevent polythionic acid SCC
The biggest issue with this is to prevent any sensitization. And I mean any. Even very light shallow areas will initiate cracking.
= = = = = = = = = = = = = = = = = = = =
Still trying to help you stop corrosion.
formerly Trent Tube, now Plymouth Tube