INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

B31.3 Restore of thickness/cosmetic repair

B31.3 Restore of thickness/cosmetic repair

B31.3 Restore of thickness/cosmetic repair

(OP)
I am looking for code based responses to this question.

Does  B31.3 address restoration of thickness of pipe (not weld metal) by addition of weld metal?

Does B31.3 address sharp edges as stress rises, or state that welds shall be free from such?

Are there any limits to restoration after hydrotest has been conducted, to a specific depth?  





RE: B31.3 Restore of thickness/cosmetic repair

WBH;
Do you have a copy of B31.3? If so, please review the following suggestions;

Review 328.6 - this also applies to base metal repairs, as is for weld metal repairs.

Review Table 341.3.2

If ANY weld repairs are required, re-hydrotest. Review 345.2.6.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources