INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Sour Water Service

Sour Water Service

Sour Water Service

(OP)
Good afternoon all,

Can anyone provide some guidelines for specifying pumps for use in sour water service?

I am looking into a 561 GPM, 280 feet of water pump that will be pumping 0.92 wt% H2S and 0.64 wt% NH3.

I am looking for any tips, but in particular for materials of construction, mechanical seal types, etc.  Thanks in advance.

RE: Sour Water Service

(OP)
Also, temperature will be 150 deg F.

RE: Sour Water Service

Nickel Development Institute Reference Book No 11 004 and NACE MR0103 will be worth consulting.

Steve Jones
Materials & Corrosion Engineer
http://www.pdo.co.om/pdoweb/

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources