Obtaining 20Ft-Lbs @ -70¦F for A537 class 1 or A516-70N
Obtaining 20Ft-Lbs @ -70¦F for A537 class 1 or A516-70N
(OP)
Has anyone been able to obtain impacts of 20Ft-Lbs @ -70°F for A537 class 1 or A516-70N in the weld and HAZ using ASME section IX, A# 1 filler metal?
Thanks for any input!
Weldmetal
Thanks for any input!
Weldmetal





RE: Obtaining 20Ft-Lbs @ -70¦F for A537 class 1 or A516-70N
RE: Obtaining 20Ft-Lbs @ -70¦F for A537 class 1 or A516-70N
For my education, will you explain why you were not req'd to reduce the temp per Table UG 84.2.
Thanks,
John
RE: Obtaining 20Ft-Lbs @ -70¦F for A537 class 1 or A516-70N
RE: Obtaining 20Ft-Lbs @ -70¦F for A537 class 1 or A516-70N