bio-based hydraulic fluid versus petro-based?
bio-based hydraulic fluid versus petro-based?
(OP)
Does anyone have experience with biodegradable hydraulic fluids and how they compare to typical petroleum based fluid when used in heavy machinery? How does their performance characteristics compare?





RE: bio-based hydraulic fluid versus petro-based?
Here is one source we used: http://www.terresolve.com/hydra.html
Some biodegradable fluids are not compatible with common petroleum system seal material. Some are. Some biodegradable fluids can be mixed with a small percentage petroleum fluid if you are replacing petroleum-based and can not remove all of it from the system.
Ted
RE: bio-based hydraulic fluid versus petro-based?
http://
Ted
RE: bio-based hydraulic fluid versus petro-based?