The main rafter and column are HyneBeam 660x85 GL17S (Australian Timber). They are reinforced with 2Y28 (or 3Y28) steel bars at top and bottom and vertical Y28 shear bars where there is a critical moment and shear. I am much appreciate if anyone experienced with it or having any brochures about the composite section can help.
Thanks.
The main rafter and column are HyneBeam 660x85 GL17S (Australian Timber). They are reinforced with 2Y28 (or 3Y28) steel bars at top and bottom and vertical Y28 shear bars where there is a critical moment and shear. I am much appreciate if anyone experienced with it or having any brochures about the composite section can help.
Thanks.






RE: Steel reinforced timber structures
Mike McCann
McCann Engineering
RE: Steel reinforced timber structures
RE: Steel reinforced timber structures
Beware that all that steel inside can cause issues with nailing.
I suggest you look up www.hyne.com.au for details.
csd
RE: Steel reinforced timber structures
What I know that I can work out the axial force in the steel bar and bond lengths of the bars using the horizontal shear strength for the timber.
I try to contact with Hyne company to get some information anyway.
RE: Steel reinforced timber structures