INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

ASTM call out for A380 Aluminum

ASTM call out for A380 Aluminum

ASTM call out for A380 Aluminum

(OP)
I need to call out the ASTM equivalent for ANSI/AA A380.0 to specify the material on a drawing.

Would "ALUMINUM ALLOY SC84A ASTM B85" be correct and/or suficient? This is for a die cast aluminum part going to Korea. We do not want to use the JIS standard ADC10 because of the higher Si content.

Where can I get an ASTM spec (for free?) to send to Korea that specifies the composition for A380.0?

RE: ASTM call out for A380 Aluminum

ASTM B 85 lists three designations for any particular alloy: one corresponding to the Aluminum Association and standardized according to ANSI H35.1, another according to ASTM B 275, and a third one that is the UNS number according to ASTM E 527.

I would use the UNS number when working with a Korean company.  For your case:

Aluminum alloy A13800 according to ASTM B 85

ASTM standards are subject to copyright laws and cannot be freely obtained.  You can purchase them from ASTM International:

http://www.astm.org

Regards,

Cory

Please see FAQ731-376: Eng-Tips.com Forum Policies for tips on how to make the best use of Eng-Tips Fora.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources