W8x17
A=5.01 in2
d=8.00 in
bf=5.250 in
tf=0.308 in
tw=0.230 in
Ix=56.6 in4
Sx=14.1 in3
rx=3.36 in
Iy=7.44 in4
Sy=2.83 in3
ry=1.22 in
rT=1.40 in
J=0.147 in4
Cw=110 in6
Zx=15.9 in3
Zy=4.36 in3