Convert silver nitrate and silver bromide into metallic silver
Convert silver nitrate and silver bromide into metallic silver
(OP)
Dear all,
Would you please suggest a chemical method for converting silver nitrate and silver bromide into metallic silver?
Thanks and best regards.
Would you please suggest a chemical method for converting silver nitrate and silver bromide into metallic silver?
Thanks and best regards.





RE: Convert silver nitrate and silver bromide into metallic silver
AgBr can be treated the same way.
Cl and Br are NOT good to inhale...
RE: Convert silver nitrate and silver bromide into metallic silver