INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Looking for the best source of conductor properties

Looking for the best source of conductor properties

Looking for the best source of conductor properties

(OP)
What is your favorite, most complete source of conductor properties?  The four properties I'm most interested in are 25°C and 50°C 60Hz resistances, the conductor GMR and the conductor outside diameter.

I've seen some fairly complete aluminum tables, but the most complete does not include GMR for single layer ACSR and we have many miles of 1/0 and 4/0 ACSR distribution neutrals underbuilt on our transmission lines.  I can find other tables that include the single layer ACSR but don't have AAC and the ACSR values differ for the other tables.  Copper conductors and copperweld shield wires need to come from other sources.

Is there a good, single source for all conductor types?  Anybody seen conductor properties for something that is similar to ACSR but where the aluminum has become fully annealed, or do the electrical properties remain the same?

Free sources would be great, but I do have access to a fair amount of other sources if there is something good to look for.

Thanks.

RE: Looking for the best source of conductor properties

Southwire has their Overhead Conductor Manual.  It's got characteristics of a variety of conductors including aluminum, ACSR and copper.

Jim Stewart and Dale Douglass of PTI did the bulk of the work on this and it's quite a good overall reference on overhead conductors.

You should be able to get a copy through a Southwire rep.

RE: Looking for the best source of conductor properties

McGraw Hill Handbook for Electrical Engineers has much of the info you are looking for.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources