INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Chrome Plating Die Cast

Chrome Plating Die Cast

Chrome Plating Die Cast

(OP)
I am wondering which material, Zinc Die Cast or Aluminum Die Cast, Chrome Plating would bound and adapt to better. Say if the part is going to be used in an outdoor grill.

RE: Chrome Plating Die Cast

Both can be satisfactorily chrome plated for outdoor decorative applications.

RE: Chrome Plating Die Cast

You're going to keep that zinc die cast part away from the hot part of the grill, right?

RE: Chrome Plating Die Cast

(OP)
the part would be on the outside of the grill say like where a company's logo would be

RE: Chrome Plating Die Cast

(OP)
my real question is which of those materials would bond to chrome plating better, in general

RE: Chrome Plating Die Cast

Zinc alloy is easier to plate and costs less to die cast (lower melting temperature) than aluminum alloy. See
FAQ about Die Casting
http://www.diecasting.org/faq/#Proper

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources