INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

filter for casutic soda

filter for casutic soda

filter for casutic soda

(OP)
Can you help me decide what type and size of filter do we need to install and use for our caustic soda (30%)considering the properties of this material. We are pumping caustic soda using 8.5 m3/hr pump in a 2-in (ID) pipe. Thanks for any advise.

RE: filter for casutic soda

Why filter it ?  What are you trying to filter ?

Store it at 20-25'C and even better keep it recirculating, and it wont need filtering ?? we do lots and lots of work with our mag-drive pumps on caustic, and do the above and all will be fine !!

www.cdrpumps.co.uk

Ash Fenn

www.cdrpumps.co.uk

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources