INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

AMS 6758 Missing Properties Data!!

AMS 6758 Missing Properties Data!!

AMS 6758 Missing Properties Data!!

(OP)
I have a requirement to weld assemblies using material IAW AMS-S-6758 "Condition C or D".
Condition C is annealed.
Condition D is normalized.  

This specification tells me that annealed (Condition C) may not be greater than Brinell 229, which I convert to HRC 21 (max) or a UTS of about 111ksi.

This spec tells me nothing about required hardness or strengths of Normalized Condition D.

Is annealed and normalized condidered to be the same??

This spec does not tell me anything about minimums either! which I will be required to demonstrate in my weld procedures. Now I can pick values out of any old handbook and other PQR tests, but I need the strength and elongation requirements to trace to the original AMS 6758 spec.
Have you been in this situation and where do you look?
Thanks if you can help.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources