We have an immediate need to obtain pricing and source a US equivalent that would meet ALL specs for 42 CrMo4V.
70mm round bar for bolt application
Yield point 750<s0.2<800 MPa - Elongation to fracture >12%
ISO - V impact test result at -40 deg C should be:
Average value over 3 samples >27J
Minimum value >70% of average value
Do you know of what US steel would meet the requirements? Is it 4140 or 4142 with Vanadium? Or is there another one?
70mm round bar for bolt application
Yield point 750<s0.2<800 MPa - Elongation to fracture >12%
ISO - V impact test result at -40 deg C should be:
Average value over 3 samples >27J
Minimum value >70% of average value
Do you know of what US steel would meet the requirements? Is it 4140 or 4142 with Vanadium? Or is there another one?





RE: 42 CrMo4V
It seems that something close is Grade B16 according to ASTM A 193/A 193M Standard Specification for Alloy-Steel and Stainless Steel Bolting Materials for High-Temperature Service.
If you need a North American source for bars, then try Republic, MACSTEEL, or Mittal:
http://www.republicengineered.com
http://www.macsteel.com
http://www.mittalsteel.com
Regards,
Cory