INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Instron TT-D XY chart drive amplifier information

Instron TT-D XY chart drive amplifier information

Instron TT-D XY chart drive amplifier information

(OP)
I have an Instron TT-D in the lab fitted with an XY chart drive amplifier.  Does anyone still have access to such a machine?  They were quite popular in the seventies but are no longer supported by the factory.  I am setting up an extensometer for training demonstrations and would like to get the XY amplifier working again.  Any information on this machine or the amplifier and how to connect it would be greatly appreciated.  We have the maintenance manuals for the rest of the machine but the XY unit is not covered by them.
Regards
Ian

RE: Instron TT-D XY chart drive amplifier information

I wouldn't waste the time and effort to make this work.  Using either Instron or a third party, I would get a digital system to condition the signals from the extensometer and the force cell.  The costs are not that great, and the headache-savings are immense.

Regards,

Cory

Please see FAQ731-376: Eng-Tips.com Forum Policies for tips on how to make the best use of Eng-Tips Fora.

RE: Instron TT-D XY chart drive amplifier information

(OP)
Thanks Cory, I agree that it is not economic to persist with the old controls and have several options for an upgrade.  I was hoping to get it working simply as a demonstration machine and to help preserve a working example of the technology of the day.  These were the last of the Instrons fitted with the old tube amps and at present it remains in totally original condition with everything working except for the output stage of the chart drive amplifier.  I was hoping someone may have an old manual or schematic lying about for the chart drive amp so we could get it working as well.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources