10B21 Material Information
10B21 Material Information
(OP)
I am looking to find out additional information on Low Carbon 10B21 material. Particularily I am looking for a document which provides the estimated tensile and yield strength of the raw material prior to processing.
Also why is the Boron added to the material. I beleive ai know but I would like some other opinions.
Thank you
Also why is the Boron added to the material. I beleive ai know but I would like some other opinions.
Thank you





RE: 10B21 Material Information
Or just have your supplier send some out for test. They dont cost but ~$100 and are easy to do. i used to work for a lab that promised A2LA certified tensiles (W/ r&n) and chemistries in under 24hours.
The boron increases the hardenability of the normally very shallow hardening 1021 carbon steel.
Nick
I love materials science!