fatigue date for Rex734 UNS 31675
fatigue date for Rex734 UNS 31675
(OP)
Currently I am looking for fatigue data for Rex 734, UNS31675 according to ASTM F1586. As far as I found there is not much data published on this material. Does anybody have a good idea where to find fatigue and other data?
Thanks
Frank
Thanks
Frank





RE: fatigue date for Rex734 UNS 31675
In a pinch you could possibly use 317L data.