INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Assembly paste in spray form

Assembly paste in spray form

Assembly paste in spray form

(OP)
We currently use Dow Corning's G-N Metal Assembly Paste and apply it with a brush. This is very time consuming. Their G-N Paste comes in a spray form, but we aren't having much success with it. The main ingredient, from what I understand, is Molybdenum Disulfide.

Are there any spray coatings available on the market that may perform better and have the same properties as the G-N paste?

Is it possible to use a thinner on the paste and run it through a spray gun? It's a pretty thick paste, somewhat like jelly.

Thanks

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources