INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

wps for welding API 5l x-65

wps for welding API 5l x-65

wps for welding API 5l x-65

(OP)
Using ANSI B31.3 and ASME sec 9 as refrence , Dose a qualified wps for weldindg API 5L-B pipe could also be used  for wlding of API 5L-X65 together?
the p no is s1 for both material , but they have different level of srength whic made me confused when I refer to note (51) of table A1 ANSI B31.3.

RE: wps for welding API 5l x-65

Quote:

Dose a qualified wps for weldindg API 5L-B pipe could also be used  for wlding of API 5L-X65 together?



Yes, without impact testing.
No, if the WPS is qualified with impact testing.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources