INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

UNS or AISI equivilent to 30MnB3

UNS or AISI equivilent to 30MnB3

UNS or AISI equivilent to 30MnB3

(OP)
Okay I have searched hi-lo for an equivalent us spec for this material listed 30MnB3...  It is used for bolts and I know its a European spec...but even when I Google it I would expect to find many hits on this material and even on matweb it has no reference to it...

Does anybody know anything about this material???

RE: UNS or AISI equivilent to 30MnB3

There is no equivalent in what you would call a US specification.  Boron-alloyed steels are more common, and have been included in more consensus standards, in Europe.  30MnB4 (you erred with 30MnB3) is included in EN 10263-4 Steel rod, bars and wire for cold heading and cold extrusion. Technical delivery conditions for steels for quenching and tempering.  Some similar documents used by US companies include ASTM F2282 Standard Specification for Quality Assurance Requirements for Carbon and Alloy Steel Wire, Rods, and Bars for Mechanical Fasteners and IFI-140 Carbon and Alloy Steel Wire, Rods, and Bars for Mechanical Fasteners.  Neither of these standards have an alloy similar to 30MnB4 - the closest are 10B21 and 10B38.

Regards,

Cory

Please see FAQ731-376: Eng-Tips.com Forum Policies for tips on how to make the best use of Eng-Tips Fora.

RE: UNS or AISI equivilent to 30MnB3

(OP)
Thanks so much, this at least can give me some more information on this particular steel...

RE: UNS or AISI equivilent to 30MnB3

What is the manganese content? If it is elevated, it might be similar to 15B30, which is similar to 30MnB5. I have never seen a 30MnB3 grade either.

RE: UNS or AISI equivilent to 30MnB3

Mn = 0.80-1.10 for 30MnB4 according to DIN EN 10263-4.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources