INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

UNI material standard

UNI material standard

UNI material standard

(OP)
Hello all.  I've got a question regarding the UNI designation of a specific steel.  We just got an Italian customer who specified the use of "52 SCN 5 UNI. S119" material.  Haven't had a chance to ask them the question yet (time difference) but this material is per the UNI standard, correct?  What is the equivalent in SAE or ASTM?  Just need to know the particulars for this material but have come up empty on the web.  Any help would be appreciated.

RE: UNI material standard

I don't believe that the UNI standard provided to you is correct.  52 SiCrNi 5 according to UNI 3545 is a spring steel grade that is alloyed with Si, Cr, and Ni.  52 SCN 5 is the old French designation according to AFNOR NF A 35.  There is no exact SAE equivalent.  The composition is similar to 9254 according to SAE J404, with somewhat lower C and some Ni added to it.  The composition is as follows:

C = 0.49-0.56
Si = 1.20-1.50
Mn = 0.70-0.90
Cr = 0.70-1.00
Ni = 0.50-0.70
P & S = 0.025 max

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources