INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

astm a694 f60

astm a694 f60

astm a694 f60

(OP)
dear all,

i cannot find mechanical properties of

ASTM A694-f60 steel

i need:

allowable stress (20°C)
yield strength (20°C)
ultimate tensile strength (20°C)
young modulus

thanks michele

RE: astm a694 f60

Per ASTM A 694/A 694M - 03 for F60...

Yeild Strength (0.2% offset): 60 ksi (415 MPa)
Tensil Strength: 75 ksi (515 MPa)

Refer to your Design Code for allowable stresses and values for young's modulus.

NozzleTwister
Houston, Texas

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources