FRP coating
FRP coating
(OP)
we are using several 11 ton and 30 year old fiberglass tanks in our processing of household products, i.e. fabric softerner, handsoap, glass cleaner, etc... We put FRP coating every 2 or 3 three years depending on the use. Is there any alternative and better coating for FRP? One time we tried putting PVC sheets in the inside, what it did not work-out. Any advice from the experts out there?





RE: FRP coating
Take a look at the Chemical Resistance Guide here:
http://www