laminate discolor Rogers4350
laminate discolor Rogers4350
(OP)
Hi, I'm sure I read somewhere that rogers 4350 can discolour "a light toast shade" is it correct that this can happen?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
laminate discolor Rogers4350
|
RE: laminate discolor Rogers4350
This stuff has a very high glass transition temperature (280 degC), much better than standard FR4.