Fittings for DIFFERENT TYPES OF STAINLESS STEEL
Fittings for DIFFERENT TYPES OF STAINLESS STEEL
(OP)
Can anybody tell me were I would get a astm number for all fittings on 316,316L 304 and 304L. I think that forgings are A182 and fittings are Astm 403 . But can somebody put me on the right track please.





RE: Fittings for DIFFERENT TYPES OF STAINLESS STEEL
The product form information below is from Table 1 in ASME B16.34, which is referenced by ASME B16.11, which is the Specification for fittings
ASTM A 182 forged/forged bar
ASTM A 240 plate
ASTM A 479 bar
ASTM A 430 Tubular
ASTM A 376 "
ASTM A 358 "
ASTM A 312 "
RE: Fittings for DIFFERENT TYPES OF STAINLESS STEEL
http://www.ssina.com/publications/specs.html
You can view, but to get a print-able copy you need to fill out a short survey. I never had any contact/spam from doing this.