Hay, in production of sheets from various polymers - mixture of MMA and fiber glasses are the ends of producted sheets unuseful. What shoul be added in the monomer mixture to prevent the oxidation or inhibition of the polymerization mixture? I am inetrested in the industrial names of added materials