Rubber Mold Releaser
Rubber Mold Releaser
(OP)
I'm looking for some tips on Rubber (NITRILE) Mold Releaser, application is Compression Molding, temp. 340 F. I'm having trouble with releasing the part (part breaks during extraction from the mold ). Need some tips on different kind of Rubber Mold Releaser that I can try (I have tried 787 & 1725L both MCLUBE and I'm looking for something better and more permanet). Any kind of suggestion on the Mold Releaser brand and proccedure is appriciated. Thank you, Genti