INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Are 317LM and 317LMN ASME approved Materials

Are 317LM and 317LMN ASME approved Materials

Are 317LM and 317LMN ASME approved Materials

(OP)
Hi Guys,

  I was wondering if 317LM (UNS S31735) and 317LMN (UNS 31726) are ASME pressure vessel code approved or recognized materials available with "SA" designations?

Bob

RE: Are 317LM and 317LMN ASME approved Materials

I did a quick review and the materials above are not listed in ASME Section II, Part D. There may be a Code Case, I will check on it.

RE: Are 317LM and 317LMN ASME approved Materials

bob330;
UNS 31726 is listed in SA 240-97. I could not find UNS 31735.

RE: Are 317LM and 317LMN ASME approved Materials

bob330,

317LM is UNS S31725.

What product form (i.e. plate, pipe, forging) are you looking for?

RE: Are 317LM and 317LMN ASME approved Materials

(OP)
Thanks Guys,

  I had a typo there......sorry. Actually I am writing a German to American alloy translation page and UNS S31725 is essentially equivalent to German alloy 1.4449.  I wanted to add a comment in my guide as to whether or not the ASME recognized all the US equivalents of the German grades.  I'm not looking for any specific form of this alloy.at least not yet.  Thanks for all the help.


    Bob

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources