Sealants for a ceramic mould
Sealants for a ceramic mould
(OP)
Hello,
I am looking for a high temperature (good to 250 deg. C) spray-on sealer for a ceramic mould, must be tough, scratch-resistant and capable of providing a vacuum seal on the mould surface. I have tried some products but with no success. Any suggestions would be very welcome. Thanks.
I am looking for a high temperature (good to 250 deg. C) spray-on sealer for a ceramic mould, must be tough, scratch-resistant and capable of providing a vacuum seal on the mould surface. I have tried some products but with no success. Any suggestions would be very welcome. Thanks.





RE: Sealants for a ceramic mould
Without more information as to the particular ceramic material and a little more on what you are trying to achieve ZYP coatings has a number of washes that might work.
http://www.zypcoatings.com/