There was an old thread on this subject (thread2-127095: Anyone have data for 7178-T6511 Aluminum?)...
I need the material properties, allowables for Aluminum Alloy 7178-T6511.
Does anyone have them? As mentioned in the old thread, apparently MIL-HDBK-5 rev D had them but I cannot get my hands on it. I have Rev J, as well as AR-MMPDS.
Any help would be most appreciated.
Thanks,
Phil
I need the material properties, allowables for Aluminum Alloy 7178-T6511.
Does anyone have them? As mentioned in the old thread, apparently MIL-HDBK-5 rev D had them but I cannot get my hands on it. I have Rev J, as well as AR-MMPDS.
Any help would be most appreciated.
Thanks,
Phil





RE: Aluminum alloy 7178-T6511
I'm pretty sure You have to get a copy of MIL-HDBK-5D [mid 1980s]. This alloy definitely disappeared from -5E.
The MIL-HDBK-5D is available thru IHS Specs and Standards.
Regards, Wil Taylor
RE: Aluminum alloy 7178-T6511
I have data from 1962 for 7178. If you want stuff that old let me have a suitably disguised e-mail address, fax or whatever, and I can send you the relevant pages.
RE: Aluminum alloy 7178-T6511
I have confirmed that a paper copy of Rev D is available from IHS ($247).
RPstress,
If you could fax the pages to 613-254-6339 that would be greatly appreciated.
Phil
RE: Aluminum alloy 7178-T6511
rec'd fax...
thanks,
Phil
RE: Aluminum alloy 7178-T6511
Phil