INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

P44 PQR / WPS Qualification

P44 PQR / WPS Qualification

P44 PQR / WPS Qualification

(OP)
I have a question I would like to have cleared up.
Scenario:
         A PQR qualified ASME SB-619 UNS N06022 to itself. The WPS reads P44 to P44 with no UNS number specified. The production material is ASME SB-619 UNS N10276. ASME IX section QW-420 provides instruction for P numbers of the same UNS grouping across the different ASME Spec. numbers but does not clarify having different UNS numbers as being the same P number.Intrepretation : IX-90-36 Question 2 appears to provde a partial answer in that a different UNS number was not allowed to be considered as the same P number to reduce PQRs. This material is being used for a lethal service and we need proper verification of the WPS.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources