AS/NZS 3992 Two thicknesses qualified in one PQR
AS/NZS 3992 Two thicknesses qualified in one PQR
(OP)
I am working with old PQR's and have come across a PQR which has 8mm, 10mm and 20mm plate qualified within the same document. All backup certs are included, but the amp input, speed and volts differ due to the different thicknesses.
Can I qualify a single WPS from 6mm - 30mm from this PQR or do the differing amps and inputs require that I split the PQR between three seperate WPS's?
Can I qualify a single WPS from 6mm - 30mm from this PQR or do the differing amps and inputs require that I split the PQR between three seperate WPS's?





RE: AS/NZS 3992 Two thicknesses qualified in one PQR
Go Freo!
RE: AS/NZS 3992 Two thicknesses qualified in one PQR
Bogu