INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Min Temp for A36 steel

Min Temp for A36 steel

Min Temp for A36 steel

(OP)
Hi,
I would appreciate if somebody can suggest a reference where min temp sustained by A36 structural steel has been given.

RE: Min Temp for A36 steel

It will depend upon thickness, stress level and type of loads.  AASHTO has some info about A36 material used at low temps.

Joe Tank

RE: Min Temp for A36 steel

SHBH;
The document TI 809-26 from the US Army Corps of Engineers, titled "Technical Instructions - Welding Design Procedures and Inspections" was available free at the time I downloaded it from the Internet, and contains information on the recommended Toughness Guidelines for Structural Steel in Fatigue Applications, Redundant Applications.

A36 is listed, and has recommended CVN impact energy requirements listed based on minimum service temperature.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources