INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

TMCP Steels - Rolling Direction

TMCP Steels - Rolling Direction

TMCP Steels - Rolling Direction

(OP)
Is it  correct to say that with TMCP steels being rolled at various temperatures and in various directions(???) - that rolling direction is no longer an issue for cold forming of a TMCP plate?

RE: TMCP Steels - Rolling Direction

Rolling direction is not as much of a concern with many steel types, now that clean steel processing has reduced inclusion contents.  The following is a nice description from Stu Keeler, forming guru:

http://archive.metalformingmagazine.com/2003/05/Science.pdf





Hard words break no bones
Fine words butter no parsnips
- my most recent fortune cookie saying

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources