SA696 Gr. B, ASME 80/S80, Sec.III
SA696 Gr. B, ASME 80/S80, Sec.III
(OP)
Hi everyone,
I already posted this same question in the B&PV forum, and got a pretty good response. I'm just curious to see what other people may suggest!
I am looking for some suggestions with a small problem I ran into with a design registration (TSSA). I completed a design report for an NC1 valve (ASME NB-3000), which was to the 1980 Edition, Summer 80 Addenda of the ASME code. Para NB 3531.1 states that B16.34 shall be used to determine the pressure-temperature ratings. As per the list of Dimensional Standards shown in Table NB-3132-1, the 1977 edition of B16.34 shall be used.
The material of the pressure boundary component being analyzed in the design report is ASME SA696 Gr.B. It is listed as a permissible material in Table I-1.0 of Section III, Division 1, Appendices. However, when using referencing B16.34-1977, we were unable to locate a material grouping which includes SA696 Gr.B. In lieu, we referenced B16.34-1981. The person at the registration authority will not register the valve because we are using the 1981 edition of B16.34, versus the 1977 edition as prescribed in ASME Div.1, Sec.III, 80/S80, Table NB-3132-1. I was hoping to dispute the fact by finding an earlier ed of B16.34 (1973) which might have included SA696 Gr.B, and saying something along the lines of:
Since SA696 Gr.B is listed in both the 1973 and 1981 editions of B16.34, by extension, the pres-temp values listed in these editions are satisfactory for analysis. But, we do not have access to the 1973 ed of B16.34 here at the office.
Any suggestions? Thanks!
I already posted this same question in the B&PV forum, and got a pretty good response. I'm just curious to see what other people may suggest!
I am looking for some suggestions with a small problem I ran into with a design registration (TSSA). I completed a design report for an NC1 valve (ASME NB-3000), which was to the 1980 Edition, Summer 80 Addenda of the ASME code. Para NB 3531.1 states that B16.34 shall be used to determine the pressure-temperature ratings. As per the list of Dimensional Standards shown in Table NB-3132-1, the 1977 edition of B16.34 shall be used.
The material of the pressure boundary component being analyzed in the design report is ASME SA696 Gr.B. It is listed as a permissible material in Table I-1.0 of Section III, Division 1, Appendices. However, when using referencing B16.34-1977, we were unable to locate a material grouping which includes SA696 Gr.B. In lieu, we referenced B16.34-1981. The person at the registration authority will not register the valve because we are using the 1981 edition of B16.34, versus the 1977 edition as prescribed in ASME Div.1, Sec.III, 80/S80, Table NB-3132-1. I was hoping to dispute the fact by finding an earlier ed of B16.34 (1973) which might have included SA696 Gr.B, and saying something along the lines of:
Since SA696 Gr.B is listed in both the 1973 and 1981 editions of B16.34, by extension, the pres-temp values listed in these editions are satisfactory for analysis. But, we do not have access to the 1973 ed of B16.34 here at the office.
Any suggestions? Thanks!