INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Slump Test For Inclined Slabs

Slump Test For Inclined Slabs

Slump Test For Inclined Slabs

(OP)
Please, I need to know what is the value of the slump test for the inclined slabs (about 33 degrees)

RE: Slump Test For Inclined Slabs

The purpose of the slump test is a measure of the flowability of the concrete.

Is this for some sort of slope protection or erosion control.

Many specifications and contractors will require lower slump concrete for proper placement and finishing of concrete on slopes. This requirement may be more restrictive than the normal concrete specifications and should be noted where it applies.

Dick

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources