INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Identify ASTM SA 387 GR D 1969

Identify ASTM SA 387 GR D 1969

Identify ASTM SA 387 GR D 1969

(OP)
Hi Everbody

A client mentioned this material ASTM SA 387 GR D - the fabrication was done in 1969. Does anybody know what is the modern equivalent of this material? Is it similar to P11 or P22? I can not find any reference in ASME II.

Thanks

IRX

RE: Identify ASTM SA 387 GR D 1969

I don't have ASME Section II at hand. All I know is back in the early 70's, the designation of SA 387 grades were changed from alphabetic to numeric. Grades were changed as...
Gr. B = Gr. 12
Gr. C = Gr. 11
Gr. D = Gr. 22
Gr. E = Gr. 21

RE: Identify ASTM SA 387 GR D 1969

(OP)
Gentlemen

Thank you to both Kenvlach and Doct9960 you gave me exactly what I was looking for

Thanks again

IRX

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources