INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

What is the major difference between MC-30 and MC-70 cutbacks?

What is the major difference between MC-30 and MC-70 cutbacks?

What is the major difference between MC-30 and MC-70 cutbacks?

(OP)
Dear Sir/Madam
I have come across some various road projects, where the medium curing grade is applied with respect to weather condition (climatically condition).This MC-30 is normally applied in moderate cold regions because of its viscous properties while MC-70 is normally preferred in hot and dry regions. In our specification require the Contractor to use MC-70 for priming works as the project road is found in dry and hot climatic condition. The Contractor is asking for a permission to use MC-30 instead of MC-70.Iwent through the testing manual (AASHTO M82-75(1993) and found that most of the properties requrement, min.and max. are same except the following tests:
Kinematic viscosity at 60Centigrade(MC-30, 30min and 60max.MC-70,70min and 140max
Distilate,percentage by volume of total distillate to 360Centigrade
Residue from distillation to 360Centigrade.
Is it possible to allow the Contractor to use MC-30 instead of MC-70 as specified? OR there will be detrimental deffect! Please assist

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources