INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Punch tooling

Punch tooling

Punch tooling

(OP)
Hi All.

I have alot of old and wornout punch and dies down here in Mexico. Does anyone know of a company that will take these off my hands for a fee and any companies that will re-grind not so badly damaged punches.

I dont have a list of tooling because there are way too many to count.

Thanks

Jon Taylor

RE: Punch tooling

If you're throwing them out, look for a scrap dealer who will give you the best price on your metal.  I don't know of any companies that buy wornout tooling from other companies so that they can re-furbish and use it.  Maybe somebody else on here does.  

Just about any tool & die shop will regrind punches for you.  It just depends on how much stock you want to take off, if you're just refacing to resharpen the detail, etc.  

Sometimes you can save pieces and rework them into others, but if space in your plant is at a premium, the 5S gods often won't allow it.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources