Invar 36 alloy (FeNi36) tensile properties
Invar 36 alloy (FeNi36) tensile properties
(OP)
Hello all!
I've just done an unsuccessful literature search for Invar36 alloy tensile props, in particular:
Young's modulus
Poisson's ratio at RT and -165 to -196°C
I need them for fracture toughness calculations. I've currently got YS and UTS data but no stress-strain curves.
Can anybody help me finding a source for these data?
Thx
I've just done an unsuccessful literature search for Invar36 alloy tensile props, in particular:
Young's modulus
Poisson's ratio at RT and -165 to -196°C
I need them for fracture toughness calculations. I've currently got YS and UTS data but no stress-strain curves.
Can anybody help me finding a source for these data?
Thx





RE: Invar 36 alloy (FeNi36) tensile properties
The company has some mechanical properties data on the website:
http://
http://www.cartech.com/index.html
Hope this helps.
Rao Yallapragada
RE: Invar 36 alloy (FeNi36) tensile properties
http://www
Try here instead;
http://www.espi-metals.com/metals/catinvar36.htm
Go the the Technical sheet for Young's Modulus
For Poisson's ratio, I would assume 0.3 for starters.
RE: Invar 36 alloy (FeNi36) tensile properties
ht
These are the guys with the most experience.
= = = = = = = = = = = = = = = = = = = =
Rust never sleeps
Neither should your protection
http://www.trent-tube.com/contact/Tech_Assist.cfm