I am trying to get material constants for a carbon fiber prepreg to be used in my PCOMP card.
The prepreg is a unitape(BMS 8 276 qualified) Toray 3900 series material made from T-800H carbon fiber. It is a 350F cure epoxy system.
I got very few properties from Toray website. Then I used COMPRO to arrive rest of the constants. I do not know all the constants are correct. I searched in internet to get right data, but no use.
Has any one got PCOMP data for this pre-preg including failure values? Appreciate, if any one shares this information or some links to find these vlaues.
Thank you..
The prepreg is a unitape(BMS 8 276 qualified) Toray 3900 series material made from T-800H carbon fiber. It is a 350F cure epoxy system.
I got very few properties from Toray website. Then I used COMPRO to arrive rest of the constants. I do not know all the constants are correct. I searched in internet to get right data, but no use.
Has any one got PCOMP data for this pre-preg including failure values? Appreciate, if any one shares this information or some links to find these vlaues.
Thank you..