INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Composite Glass Stair Tread

Composite Glass Stair Tread

Composite Glass Stair Tread

(OP)
I have a composite glass stair tread supported at the corners with the following layers:
8mm Annealed Glass
1.52mm DuPont SentryGlas Plus Interlayer
15mm Annealed Glass
1.52mm DuPont SentryGlas Plus Interlayer
15mm Annealed Glass
1.52mm DuPont SentryGlas Plus Interlayer
8mm Annealed Glass
Total Thickness=50.56mm

What is the best way to analyze this composite material? Is there particular programs that are required to analyze this? Any help on this matter would be appreciated.

Thank you,

Val Courtney, PE
Valstone Engineering, Inc.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources