INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Thread specifications

Thread specifications

Thread specifications

(OP)
I need to know the dimensions for a 9/16 - 18 SAE Port Thread. Where can I find this info or, does anyone have the dimensions, such as Major, Minor and Pitch diameters, any lead taper, etc? Thanks in advance for the help!

RE: Thread specifications

Is this a straight thread tube fitting boss? If so the thread is 9/16-18UNF-3B.

RE: Thread specifications

Did you check in the Machinery's Handbook?

Thanks!
Pete
P. J. (Pete) Chandler, PE
Principal Engineer
Mechanical, Piping, Thermal, Hydraulics
Processes Unlimited International, Inc.
Bakersfield, California USA
pjchandl@prou.com

RE: Thread specifications

Actually, the thread is a 9/16-18UNF-2B.  Thread Pitch diameter is between .5264 & .5323; minor thread diameter is between .502 & .515

RE: Thread specifications

Depends on the spec., MS33649 calls for 3A/3B.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources