Material Suggestions
Material Suggestions
(OP)
I would like to get some suggestions on a material for a container for transport. I am no materials engineer, so some input would be greatly appreciated. The material doesn't necessarily have to be a metal, it could be a composite, plastic, polymer or other. The main spec is that it has to withstand a fire penetration test of 1,700°F for 5 minutes. I am looking for a good insulator that would keep the contents cool as well. Any suggestions?





RE: Material Suggestions
RE: Material Suggestions
There are standard fire resistant desings out there.
= = = = = = = = = = = = = = = = = = = =
Rust never sleeps
Neither should your protection
http://www.trent-tube.com/contact/Tech_Assist.cfm