1965 18J6 Steel Joist Capacity
1965 18J6 Steel Joist Capacity
(OP)
I'm working on a building constructed in 1965 that has 18J6 steel joists spanning 27 feet. Does anyone have a table from that time-frame that indicates what the capacity of the joist is?






RE: 1965 18J6 Steel Joist Capacity
http://www.steeljoist.org/publications/default.asp
www.SlideRuleEra.net
RE: 1965 18J6 Steel Joist Capacity
RE: 1965 18J6 Steel Joist Capacity
RE: 1965 18J6 Steel Joist Capacity
Total allowable uniform=268 lb/ft and Fy=22 ksi