INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

new concrete slab over existing slab

new concrete slab over existing slab

new concrete slab over existing slab

(OP)
i hope someone can help

we want to pour a new concrete slab 5" thick rienfoced with 2" fibermesh on top of an existing slab.we are thinking of placing poly on top of the existing slab so the two slabs are isolated.the existing floor is 6" thick,over 50 years old and has a lot of surface wear.New slab is 15,000 sq. ft. and would be sawcut into 15' squares.New floor will have forklift traffic on it.There are 6 areas 6' x 6' that are broken areas and we want to install re bar mats in these areas without removing the dameged concrete.

your help would be greatly appreciated.
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources