INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

AlZnMgCu 1.5F48 callout ???

AlZnMgCu 1.5F48 callout ???

AlZnMgCu 1.5F48 callout ???

(OP)
I have a drawing that calls out an aluminum spec. of AlZnMgCu 1.5F48.

Does anyone know of a comparable U.S. material specification??

RE: AlZnMgCu 1.5F48 callout ???

I am not sure what F48 stands for.  

DIN 17007: 3.4365
AA:7075
ISO: Al-Zn-MgCu
NF A02-004: AZ- 5GU
BS/BS-L: 2L 95/96
UNI: P-AlZn5.8MgCu
ALCAN: 75S
 
or go to the following website:
http://www.astrosurf.com/altaz/alu.htm

Rao Yallapragada

RE: AlZnMgCu 1.5F48 callout ???

The F48 indicates the desired ultimate tensile strength of the end product in MPa, multiplied by 0.1.  In this case, 480 MPa.  It is an obsolete designation from DIN 17007.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources