INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Shot Peening

Shot Peening

Shot Peening

(OP)
Is there any data avalable on shot peening intensity vs residual stress measurements?

RE: Shot Peening

No.Intensity depends on shot size, velocity, coverage and peening time.Thus,you can obtain the same Almen strip intensity in different ways. The residual stress pattern that a shot peening process of any given intensity will produce will vary with material hardness.

RE: Shot Peening

The residual stress pattern after shot peening is also highly dependent on the previous stresses within the part.  Lots of information available from Metal Improvement or shotpeener.com.

RE: Shot Peening

I have had stuff shot peened by Metal Improvement.  Those folks know their business.  They better; lots of aircraft, particularly helicopters fly stuff they peened.

But...you need to know what it is that you are after in order to give them a starting place.

rmw

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources